Hi folks,

I've been using the above on my current project (model aircraft) and have been impressed with it's hardness when cured. But I find it's quite thick to brush on and doesn't flow very well, leaving quite an irregular surface .  Is it possible to thin it slightly so that it flattens out better?




Many thanks, Marty
Reply
FLD
FLD
Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)
Group: Forum Members
Posts: 468, Visits: 2.7K
I wouldn't recomend it.  Can I ask why you need to use epoxy tooling gel?  I currently use polyester tooling gel and I find that cures to a nice, hard, polishable surface. This stuff.  I use it for all laminates without problems.
Edited 12 Years Ago by FLD