Hi,
The part is around 1800mm x 800mm x 40mm. I am going to try to design the infusion by doing the front and the back in separate steps.
I need to try to come up with a way of creating a join around the 40mm edge, Ill have to research this a little further but I will post results once I manage to get things moving :-)
|