Group: Forum Members
Posts: 2.5K,
Visits: 28K
|
You've got to be using wayyyyy too much. When I use it, I can barely see it on the mould surface. I put the mould down on the ground and give the adhesive a very quick spray from a meter above it, let the mist settle down on it. Works like like a charm, doesn't leave any residue on the surface and epoxy has no problems with it.
|