Residue issues on mould. Spraymount the cause?

http://www.talkcomposites.com/Topic11717.aspx

By brettalloy - 6/9/2014 8:06:00 AM

Morning guys,

Please see my pics attached, imp having a problem withresidue being left in mould and making parts stick.

I believe it’s the spray mount I use to tack cloth in placeon the mould. I don’t use a lot but I’m thinking I won’t use any tack spray andlet the bag pull cloth into position.

Been using 3m re position able photo mount spray.

Does the epoxy resin react to this spray??

As sometimes resin has been left in the mould when I pulledparts out leaving me some porosity in the surface.

By Warren (Staff) - 6/10/2014 2:32:11 PM

That does seem like classic case of too much spray tack.  Less is better!