Hello,

As I'm new in carbon fiber, I'm wondering about the ratio 100:30 which is printed on the containers , what does mean, if there is any example please?
Reply
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
If you are not sure, just keep it simple and mix in batches of 100g of resin.  That way for every 100g of resin, you need 30g of hardener.  Simple enough to do in your head and be confident youve got it right.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search