Epoxy resin Ratio 100:30


Author
Message
Salim
Salim
Forum Guru (67 reputation)Forum Guru (67 reputation)Forum Guru (67 reputation)Forum Guru (67 reputation)Forum Guru (67 reputation)Forum Guru (67 reputation)Forum Guru (67 reputation)Forum Guru (67 reputation)Forum Guru (67 reputation)
Group: Forum Members
Posts: 3, Visits: 40
Hello,

As I'm new in carbon fiber, I'm wondering about the ratio 100:30 which is printed on the containers , what does mean, if there is any example please?
Reply
brainfart
brainfart
Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)
Group: Forum Members
Posts: 198, Visits: 1.4K
Oops, for the last three I accidentially picked the same example. Sorry.

Yes seems to be right.