Hi there,

I'm using your EL2 and I hope if you can help me to find some of EL2 thermal properties namely: Conductivity,  specific heat, and coefficient of thermal expansion.

Thanks

Mohamed
Reply
noble350
noble350
Supreme Being (95 reputation)Supreme Being (95 reputation)Supreme Being (95 reputation)Supreme Being (95 reputation)Supreme Being (95 reputation)Supreme Being (95 reputation)Supreme Being (95 reputation)Supreme Being (95 reputation)Supreme Being (95 reputation)
Group: Forum Members
Posts: 11, Visits: 131
Thanks, but unfortunately it doesn't contain the properties that I listed above!