noble350
noble350
posted 12 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 11,
Visits: 131
Hi there,
I'm using your EL2 and I hope if you can help me to find some of EL2 thermal properties namely: Conductivity, specific heat, and coefficient of thermal expansion.
Thanks
Mohamed
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Thermal properties of epoxy resin EL2
noble350
-
12 Years Ago
All the tech data is on the EC site....
carbonfibreworks
-
12 Years Ago
Thanks, but unfortunately it doesn't contain the properties that I listed above!
noble350
-
12 Years Ago
The properties you are after don't exist as they haven't been measured by the manufacturer. They are...
Warren (Staff)
-
12 Years Ago
Hi Warren, I need these properties for reserach sake. I used EL2 to made CFRP bars, which I put...
noble350
-
12 Years Ago
If you find that kind of data for other epoxy resins you can use those numbers as an approximation....
brainfart
-
12 Years Ago
Unfortunately in literature data is scarce and conflicting.
noble350
-
12 Years Ago
If you are doing this as a uni project and with lab work then find out the testing procedure for...
ChrisR
-
12 Years Ago
No doubt there are established ASTM/DIN/whatever procedures for such testing. And Chris is right,...
brainfart
-
12 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search