So, i accidentally grabbed a small bottle of resin IN2 instead if hardener (SLOW) when my hardener bottle ran out and completed the mix with more resin. Ive ended up with a mold with resin in it thats only got half the hardener in it it should have. Shall i bin it all now or is it worth waiting? and waiting ....

Thanks

Ben
Reply
benet
benet
Supreme Being (547 reputation)Supreme Being (547 reputation)Supreme Being (547 reputation)Supreme Being (547 reputation)Supreme Being (547 reputation)Supreme Being (547 reputation)Supreme Being (547 reputation)Supreme Being (547 reputation)Supreme Being (547 reputation)
Group: Forum Members
Posts: 59, Visits: 373
4 days later and the resin is still not cured. tacky, thick , but not at all cured.. Binned - lesson learned i hope.,