By benet - 5/9/2014 10:10:25 AM
So, i accidentally grabbed a small bottle of resin IN2 instead if hardener (SLOW) when my hardener bottle ran out and completed the mix with more resin. Ive ended up with a mold with resin in it thats only got half the hardener in it it should have. Shall i bin it all now or is it worth waiting? and waiting ....
|
By benet - 5/12/2014 10:56:52 AM
4 days later and the resin is still not cured. tacky, thick , but not at all cured.. Binned - lesson learned i hope.,
|
|