Hi,

So basically I don't really want to make a mould of the center console of my car.

I was hoping of simply wrapping the carbon fiber around it, but applying a release agent to it and not tucking it under the edges so I can pop it out from under it.

Do maybe 3 layers of 2/2 twill CF then do one final layer and do a few coats of epoxy resin. A bit like the skinning process, but using epoxy resin instead of epoxy coating?

Would this work? The piece is pretty simple. I could get a picture of the parts I plan to do!

Cheers
Reply
Matthieu Libeert
Matthieu Libeert
Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
should work well but the fit might give some problems...you'll ADD some thickness compared to the original part so might keep that in mind Wink

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search