Technical Support (1.4K reputation)Technical Support (1.4K reputation)Technical Support (1.4K reputation)Technical Support (1.4K reputation)Technical Support (1.4K reputation)Technical Support (1.4K reputation)Technical Support (1.4K reputation)Technical Support (1.4K reputation)Technical Support (1.4K reputation)
Group: Administrators
Posts: 134, Visits: 614
Hi,

If you sand the surface of the GRP really well you should be able to achieve a really good bond with just the resin, so it wouldn't be essential to use the basecoat, however if the part is not already black the basecoat will help by ensuring that the tiny gaps between the weave don't show through. 

Paul Statham
Easy Composites / Carbon Mods - Technical
joey54321
joey54321
Forum Guru (70 reputation)Forum Guru (70 reputation)Forum Guru (70 reputation)Forum Guru (70 reputation)Forum Guru (70 reputation)Forum Guru (70 reputation)Forum Guru (70 reputation)Forum Guru (70 reputation)Forum Guru (70 reputation)
Group: Forum Members
Posts: 6, Visits: 27
HI,

I have made a part out of fibreglass and looking to 'skin' it in Carbon. Will I need the basecoat or will a layer of resin between the fg and the cf be adequate?



Thanks
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search