Mould cleaning query


Author
Message
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
Mould cleaner will work  great but will remove all trace of release agents.  Same with Acetone.  A wipe of acetone over the surface of a fully cured seasoned mould shoudn't cause any problems but mould cleaner is the better choice if its available to you.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
brettalloy
brettalloy
Supreme Being (145 reputation)Supreme Being (145 reputation)Supreme Being (145 reputation)Supreme Being (145 reputation)Supreme Being (145 reputation)Supreme Being (145 reputation)Supreme Being (145 reputation)Supreme Being (145 reputation)Supreme Being (145 reputation)
Group: Forum Members
Posts: 23, Visits: 69
Thanks will try this and hopefully wont have to resort to more aggressive methods!
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Soap and warm water is all it takes to clean mine up. I always treat it as a new mould then, and reapply the release agent as if it never had been.
brettalloy
brettalloy
Supreme Being (145 reputation)Supreme Being (145 reputation)Supreme Being (145 reputation)Supreme Being (145 reputation)Supreme Being (145 reputation)Supreme Being (145 reputation)Supreme Being (145 reputation)Supreme Being (145 reputation)Supreme Being (145 reputation)
Group: Forum Members
Posts: 23, Visits: 69

Ive made about 5 parts out of my mould via infusion. Someparts didn’t work, combination or porosity, poor consolidation, mixing.

Anyway i have a film or build up on mould surface.

 

Easylease does a fairly good job of cleaning up but still aresidue remains.

 

Do i remove this with acetone, or a mould cleaner.

I was thinking acetone be good to strip it all off, providedi then put a good easylease coat back on.

 

Im wondering wether this residue will not come off with astandard mould cleaner.

 

Cheers Brett