Ive made about 5 parts out of my mould via infusion. Someparts didn’t work, combination or porosity, poor consolidation, mixing.
Anyway i have a film or build up on mould surface.
Easylease does a fairly good job of cleaning up but still aresidue remains.
Do i remove this with acetone, or a mould cleaner.
I was thinking acetone be good to strip it all off, providedi then put a good easylease coat back on.
Im wondering wether this residue will not come off with astandard mould cleaner.
Cheers Brett