Morning all,

I am hoping to move from using epoxy resins and polymer clays to casting for the claws on my hand sewn sloths and bears.  I have cast a few parts in resin before at University but it was a while ago and under supervision of an artist, so I don't have a clear idea of the direction the claws would be best sitting in the mould.  I don't know if this needs to be a two part mould with the claws lying horizontally or vertically, or if the silicone is flexible enough that I could just have a single layer with the mould creeping over the top of the claw but a small space to fill from.  I assume the holes will complicate things further too.

Anyway, any advice before I take the plunge is much appreciated; I hope the attached images of the claws in use and how I think they could be cast are helpful, but I have no doubt they could be completely wrong!

Thanks,

Chloe.

http://www.talkcomposites.com/Uploads/Images/c496d57b-3b5a-40f9-94ee-dafe.jpg   http://www.talkcomposites.com/Uploads/Images/c229db39-6682-4adb-be47-3d33.jpg
Hanaldo
Hanaldo
Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
I'd say there's a couple of ways to go about it, just depends on what you actually need. The easier, but less accurate/detailed way would be to do a simple blanket mould. Lay the claw flat on a piece of plastic, stuck down with a tiny bit of hot glue, then brush some silicone over it in a few layers. 

I think the better way though, would be to do a 2 part block mould. This video gives a great walkthrough on how to do it: 

https://www.youtube.com/watch?v=YGZ2OeQinzw

If you did it that way, with the claw pushed halfway into the clay then you shouldn't have any issues with the hole at the end.
Gantaeno
Gantaeno
Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)
Group: Forum Members
Posts: 2, Visits: 10
Thank you for the link, that's a great help and I can see how that would work with the claws as well.  This is the method we used at University, but I had forgotten the use of clay completely: no wonder it wasn't making sense!

Thanks again  Smile
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search