Just a quick one regarding epoxy adhesives in cartridges and their applicator guns:

Is there anything stopping me from NOT using the static mixer nozzles? So just using the cartridge and discharging a small amount, then mixing it and applying it myself? 
carbonfibreworks
carbonfibreworks
Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)
Group: Forum Members
Posts: 292, Visits: 4.5K
Hi Hanaldo
Yes it is OK to use your method, i only use mixer nozzles when working on a big job.
Regards Chris
carbon fibre works LTD

http://www.talkcomposites.com/Uploads/Images/97e08777-693c-4af1-a27a-86cf.png
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Perfect, thanks Chris. 

The mixer nozzles are $5 each here, would need to use my left arm as down payment :glare:
carbonfibreworks
carbonfibreworks
Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)
Group: Forum Members
Posts: 292, Visits: 4.5K
Your welcome
 You need the gun/dispenser to ensue you have equal amounts , you could do it without but when mixing small amounts it is not worth the risk.
Chris
Carbon fibre works LTD 

http://www.talkcomposites.com/Uploads/Images/97e08777-693c-4af1-a27a-86cf.png
FLD
FLD
Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)
Group: Forum Members
Posts: 468, Visits: 2.7K
The nozzles are a quid each here and I still use that approach for small amounts.  Works perfectly! 
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Yes the nozzles work very well, but I need to dispense it onto a piece of plastic so that I can mix some pigment in before applying it, so I would end up applying it with a brush anyway. Big waste of an expensive mixer to do it that way.