Our ProFinishCarbon Fibre 2/2 Twill has an uncured resin binder on it so when you infuse or wetlay, it cures and cross-link polymerises with the epoxy resin system being used.

That means you are highly unlikely to notice any surface difference whichever way up you use the material.


Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
ajb100
ajb100
Supreme Being (4.4K reputation)Supreme Being (4.4K reputation)Supreme Being (4.4K reputation)Supreme Being (4.4K reputation)Supreme Being (4.4K reputation)Supreme Being (4.4K reputation)Supreme Being (4.4K reputation)Supreme Being (4.4K reputation)Supreme Being (4.4K reputation)
Group: Forum Members
Posts: 346, Visits: 4.4K
the binder will be surrounded by the resin when used and be made invisible.

as with you, ive used it both sides up and never found any defects. its gotton to the point now were i dont look at what side im putting face down
andygtt
andygtt
Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)
Group: Forum Members
Posts: 157, Visits: 1.2K
on a related note.... its mentioned that pro finish is sided i.e. 'there is a light splattering of resin on the rear'.

Im using profinish on large parts and am having to use it both sides up, so the "rear" of the profinish is on the surface of the part on half the part.... i've not noticed any difference in finish once the part is made although there is a difference when viewing the cloth itself prior to resin applied, but is there a reason not to use the rear side as a finished side?
Matt (Staff)
Matt (Staff)
Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)
Group: Forum Members
Posts: 680, Visits: 1.9K
Warren is totally right, ProFinish should be used in exactly the same way as you would use a dry carbo cloth which is that it can be cured at ambient temperature, laminated using wet lay, vacuum bagging, infusion, RTM etc. The resin 'spattering' on the reverse is very faint and dissapears once the resin goes through.

--Matt

Matt Statham
Easy Composites / Carbon Mods - Technical Sales
TPerino
TPerino
Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)
Group: Forum Members
Posts: 2, Visits: 30
Thanks for the help.  I look forward to trying it and seeing the end results.

Thanks again!
Warren
Warren
Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)
Group: Administrators
Posts: 214, Visits: 783
From what i understand about the pro finish, it is a normal cloth with a light splattering of resin on the rear, which when it cures during manufacture, helps hold the weave together and avoid fraying when you the customer uses it.

I dont see why it wouldnt cure at room temperature.  Ive used profinish in resin infusion cured at room temperature with no problems.
TPerino
TPerino
Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)
Group: Forum Members
Posts: 2, Visits: 30
I love the idea of the ProFinish cloth used for the surface layer of a part.

My question is- Can you air cure when using a ProFinish surface layer on a wet lay-up?

I do a lot of wet lay-up parts (all under full vacuum) in an oven. But some parts are to large for our current oven.

This is a side business at home. But I work for a aerospace company(GKN North America) and have 10+ years of experience using autoclave and non autoclave pre-preg. Also air cured part when doing a new part or tool mockup. So using a "pre-preg like" cloth, outside of an oven, if a little foreign to me.

Thank you in advance. You have a great site.

Tom
Edited 14 Years Ago by TPerino
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search