By TPerino - 3/18/2012 4:15:50 PM

I love the idea of the ProFinish cloth used for the surface layer of a part.

My question is- Can you air cure when using a ProFinish surface layer on a wet lay-up?

I do a lot of wet lay-up parts (all under full vacuum) in an oven. But some parts are to large for our current oven.

This is a side business at home. But I work for a aerospace company(GKN North America) and have 10+ years of experience using autoclave and non autoclave pre-preg. Also air cured part when doing a new part or tool mockup. So using a "pre-preg like" cloth, outside of an oven, if a little foreign to me.

Thank you in advance. You have a great site.

Tom
By Warren (Staff) - 3/20/2013 12:39:06 PM

Our ProFinishCarbon Fibre 2/2 Twill has an uncured resin binder on it so when you infuse or wetlay, it cures and cross-link polymerises with the epoxy resin system being used.

That means you are highly unlikely to notice any surface difference whichever way up you use the material.