Hey there,

Just been experimenting with the Silicone Mould Resin Casting Kit and have achieved good results so far, but I do have a question regarding the Silicone curing time:

Is there any way to speed it up?

I've seen online places that suggest increasing the ratio of silicone to catalyst from 100:5/20:1 to something a little higher, but obviously the pot says 100:2-5 and I don't want to go overboard and end up with something that is unusable!

Thanks for your time,
Paul
Reply
Matthieu Libeert
Matthieu Libeert
Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
I've worked with some other silicones and time was cut by half or more while using heated environment... you mix everything at room temperature and pour it on the part then put everything in the oven at 60°C. Make sure you dont use your normal oven you use every day to cook with Wink it's still a chemical mixture. 

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search