Hello

guys i be making full widebodykit for me. can anyone suggest how many layers and what to put best so to be good in weight also to be strong and not to flexible.

Bodykit be made from fiberglass.

1.front bumper
2. front fenders set
3. hood
4. side skirts set
5. doors skins set
6. rear fenders set
7. rear bumper
8. canards set
9. wing
10. wing extra small one 
Reply
TomDesign
TomDesign
Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)
Group: Forum Members
Posts: 454, Visits: 2.5K
my wing is from 9 pieces Smile guys i go normal way as i used budget molds and guy made me but without flanges so i can not do infusion . i think i go with 300gr 3 layers or  1 layer 300 and 6 6oogrnad i put hard foarm before last layer so parts get structural stable things.

as for all bodykit i calculated need around 70 kg resin polyster and 40 sq metres frp. plus gelcoat.
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
TomDesign - 11 Years Ago
ajb100 - 11 Years Ago
ChrisR - 11 Years Ago
TomDesign - 11 Years Ago
The Fibreglass King - 11 Years Ago
The Fibreglass King - 11 Years Ago
TomDesign - 11 Years Ago
matthieutje65 - 11 Years Ago
TomDesign - 11 Years Ago
The Fibreglass King - 11 Years Ago
wozza - 11 Years Ago
wozza - 11 Years Ago
combustioncraig - 11 Years Ago
wozza - 11 Years Ago
TomDesign - 11 Years Ago
TomDesign - 11 Years Ago
wozza - 11 Years Ago
TomDesign - 11 Years Ago
wozza - 11 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search