Hello

guys i be making full widebodykit for me. can anyone suggest how many layers and what to put best so to be good in weight also to be strong and not to flexible.

Bodykit be made from fiberglass.

1.front bumper
2. front fenders set
3. hood
4. side skirts set
5. doors skins set
6. rear fenders set
7. rear bumper
8. canards set
9. wing
10. wing extra small one 
Reply
wozza
wozza
Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)
Group: Forum Members
Posts: 688, Visits: 5.4K
Found a picture of  a nose section I did for a historic BRM using the above lay up. The nose is 2m x 1.9m and plenty strong enough and low weight (compared with the original).

Warren

Carbon Copies Ltd
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
TomDesign - 11 Years Ago
ajb100 - 11 Years Ago
ChrisR - 11 Years Ago
TomDesign - 11 Years Ago
The Fibreglass King - 11 Years Ago
The Fibreglass King - 11 Years Ago
TomDesign - 11 Years Ago
matthieutje65 - 11 Years Ago
TomDesign - 11 Years Ago
The Fibreglass King - 11 Years Ago
wozza - 11 Years Ago
wozza - 11 Years Ago
combustioncraig - 11 Years Ago
wozza - 11 Years Ago
TomDesign - 11 Years Ago
TomDesign - 11 Years Ago
wozza - 11 Years Ago
TomDesign - 11 Years Ago
wozza - 11 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search