about aluminium honeycomb. how does this work when being used with carbon infusion? i mean in the sandwich are the carbon sheets just glued with resin either side?
ajb100
ajb100
Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)
Group: Forum Members
Posts: 346, Visits: 4.4K
Most use an adhesive to hold it together as resin is too viscous so won't always reach in all places
coleio
coleio
Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)
Group: Forum Members
Posts: 68, Visits: 285
how is it done then? does the aluminium collapse? it really baffel me lol. also i heard that carbon fibre and aluminium react badly?
ajb100
ajb100
Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)
Group: Forum Members
Posts: 346, Visits: 4.4K
You use a structural adhesive to bond it together.

The aluminium doesn't collapse, it's what creates the gap between the carbon layers giving it the rigidity

Yes they do react, it's called galvanic corrosion
coleio
coleio
Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)
Group: Forum Members
Posts: 68, Visits: 285
whats the process then? im guessing its not done during the resin infusion process? because i saw omeones project where he used some sort of honeycomb core during infusion, so im wondering what way the resin gets sucked through, filling the fibres but not the honeycomb structure??

for the alu are the carbon panels bade seperately and then added to the honeycomb once cured? whats done to prevent corrosion? 
Matthieu Libeert
Matthieu Libeert
Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
The way I would do it is make the part this way:
Lay your lay-up in the mould and infuse (no honeycomb)
Let it cure and remove vac-bag materials and peelply
Add resin on that layer and put your honeycomb on it
Add some vacuum to firmly bond the honeycomb on that first layer
Wet lay toplayer on a serpearate sheet and put it on top of honeycomb and vacuumbag again

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search