Hi there.

I'm going to be constructing a complex shape with the external cosmetic layer of reinforcement being red CF. I've worked out how to cut almost the entire shape as a single large piece (140cm x 70cm to give a rough idea of scale), and with all the cuts being perpendicular to minimise issues with fraying.

However that's not quite perfect, and the item will need two rather more fiddly small pieces to complete, with really precise cuts at odd angles. The concern is that fraying will be impossible to avoid and that those bits will spoil an otherwise perfect cosmetic part. Is there a trick here?

Can I spray a small piece with some sort of glue before cutting that will keep it together without any fraying, and are there any particular pitfalls to look out for to avoid spoiling the cosmetic appearance.

Thanks in advance.
carbonfibreworks
carbonfibreworks
Supreme Being (3.8K reputation)Supreme Being (3.8K reputation)Supreme Being (3.8K reputation)Supreme Being (3.8K reputation)Supreme Being (3.8K reputation)Supreme Being (3.8K reputation)Supreme Being (3.8K reputation)Supreme Being (3.8K reputation)Supreme Being (3.8K reputation)
Group: Forum Members
Posts: 292, Visits: 4.5K
You can use a light mist of Aerofix 3 to spray the back .
Chris
www.carbonfibreworks.co.uk

http://www.talkcomposites.com/Uploads/Images/97e08777-693c-4af1-a27a-86cf.png
Matthieu Libeert
Matthieu Libeert
Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
What Chris says is correct,
Use a composites spray glue, give it a quick spray on the line you plan to cut and it will prevent any fraying. 
Or you could use some painters tapeto have a nice cut

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




ajb100
ajb100
Supreme Being (4.4K reputation)Supreme Being (4.4K reputation)Supreme Being (4.4K reputation)Supreme Being (4.4K reputation)Supreme Being (4.4K reputation)Supreme Being (4.4K reputation)Supreme Being (4.4K reputation)Supreme Being (4.4K reputation)Supreme Being (4.4K reputation)
Group: Forum Members
Posts: 346, Visits: 4.4K
One issue I've had in the past with spraying glue on the fabric to avoid fraying is that it also significantly reduces the drape of the fabric, so if it's a complex shape, be careful to only spray where you are going to cut, and lightly too
KeyboardWarrior
KeyboardWarrior
Supreme Being (100 reputation)Supreme Being (100 reputation)Supreme Being (100 reputation)Supreme Being (100 reputation)Supreme Being (100 reputation)Supreme Being (100 reputation)Supreme Being (100 reputation)Supreme Being (100 reputation)Supreme Being (100 reputation)
Group: Forum Members
Posts: 4, Visits: 14
Thanks very much for the helpful replies. I'll give it a go and spray carefully.Smile
Toffee
Toffee
Supreme Being (480 reputation)Supreme Being (480 reputation)Supreme Being (480 reputation)Supreme Being (480 reputation)Supreme Being (480 reputation)Supreme Being (480 reputation)Supreme Being (480 reputation)Supreme Being (480 reputation)Supreme Being (480 reputation)
Group: Forum Members
Posts: 36, Visits: 118
I would add, just a little spray as advised but then leave for a short while until the area loses its tackiness, it can start sticking everywhere otherwise.
carbon Booms
carbon Booms
Forum Member (43 reputation)Forum Member (43 reputation)Forum Member (43 reputation)Forum Member (43 reputation)Forum Member (43 reputation)Forum Member (43 reputation)Forum Member (43 reputation)Forum Member (43 reputation)Forum Member (43 reputation)
Group: Forum Members
Posts: 1, Visits: 2
I have a technique that I use to put a very thin layer of toilet tissue onto the carbon mat.  You will see it all here:

https://www.youtube.com/watch?v=RGLoA0hP2jY

There is a change to the technique shown here, though. When the tissue gets damp it expands.  Now after I have laid the dry tissue onto the carbon mat I damp it slightly so it expands and then very gently pull the wrinkles out.

Please be aware that PVA can stop the carbon from bonding, so it may weaken your product slightly.  I have never had any problems, myself.