Can anyone comment on the differences between 3D core and Soric  both from easy composites? They appear fairly similar....
Reply
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
What they said.

the difference is clearer with the products side by side.

http://www.talkcomposites.com/Uploads/Images/685ad845-2282-4b02-919d-c9f5.jpg

The cells on 3D core are much bigger relative to Soric.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search