jamesw
jamesw
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 61,
Visits: 558
Thanks all - got it
James
Reply
Like
10
Warren (Staff)
Warren (Staff)
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Administrators
Posts: 2.5K,
Visits: 8.5K
What they said.
the difference is clearer with the products side by side.
The cells on 3D core are much bigger relative to Soric.
Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Reply
Like
11
FLD
FLD
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 468,
Visits: 2.7K
As said 3d core has much less resin uptake (its basically hexagons of foam). There is greater print through with 3d core though and it also isn't quite as conformable.
Reply
Like
12
ajb100
ajb100
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 346,
Visits: 4.4K
From my understanding of it, it's the resin uptake that sets them apart, the 3d core uses much less resin meaning a lighter finished item
Reply
Like
10
jamesw
jamesw
posted 12 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 61,
Visits: 558
Can anyone comment on the differences between 3D core and Soric both from easy composites? They appear fairly similar....
Reply
Like
11
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
11
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search