Is there a good way to get carbon to go tightly round a right angle?

Thanks
Reply
Warren
Warren
Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)
Group: Administrators
Posts: 214, Visits: 783
Just remember if you cut down the corners, you will need on the structural layers to cut it differently so it doesnt just break on the corners. eg wrap a length of carbon around the 4 sides then use a blob spray tack to hold it.

better still, use a long tow of carbon to in effect tie around the box rather than glue.  it will lay flat nicely and not effect cosmetic finish.

You will find it much easier to use profinish carbon when doing complicated cuts as the edges of normal carbon will fray easily looking messy.

ideally pre-preg would suit such a part as it is sticky so would cut nicely and hold itself in position while you lay up.  However i understand cost may be prohibitative.
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
joey54321 - 14 Years Ago
Joe - 14 Years Ago
joey54321 - 14 Years Ago
Warren - 14 Years Ago
joey54321 - 14 Years Ago
Joe - 14 Years Ago
Warren - 14 Years Ago
Matt (Staff) - 14 Years Ago
joey54321 - 14 Years Ago
Paul (Staff) - 14 Years Ago
CarbonMike - 14 Years Ago
Matt (Staff) - 14 Years Ago
CarbonMike - 14 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search