joey54321
joey54321
posted 14 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 6,
Visits: 27
Is there a good way to get carbon to go tightly round a right angle?
Thanks
Reply
Like
11
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Carbon cloth and right angles
joey54321
-
14 Years Ago
Hi. If you use vacuum, it will help. But as always you will need to massage the bag with some tool...
Joe
-
14 Years Ago
Where would you place the cuts? It is the the outside I was thinking of and don't have access to a...
joey54321
-
14 Years Ago
without a vacuum pump it will be tough to keep the carbon in position. you could make a (blunt)...
Warren
-
14 Years Ago
I wish I could afford a vacuum pump :(. I guess I will have to try and get a few right angle to...
joey54321
-
14 Years Ago
Hey, Dont forget the spray glue, it could really help you in a non-vacuum process. i have no idea...
Joe
-
14 Years Ago
Just remember if you cut down the corners, you will need on the structural layers to cut it...
Warren
-
14 Years Ago
Warren's right that ProFinish might help you a lot in getting a good cosmetic finish on right angled...
Matt (Staff)
-
14 Years Ago
I have just been informed that ourinflatablebed inflater actually has a vacuum/deflate mode. While I...
joey54321
-
14 Years Ago
Hi Joey, Your right in thinking that an air-bed deflator would not have anything like the level of...
Paul (Staff)
-
14 Years Ago
Sorry to bump an old thread.... But... this was made via wetlay, using no cuts nor no vac setup,...
CarbonMike
-
14 Years Ago
Hi Mike, You've done well there, especially considering it's a 650g cloth you're using which is...
Matt (Staff)
-
14 Years Ago
[quote][b]Matt (Staff) (17/06/2012)[/b][hr]Hi Mike, You've done well there, especially considering...
CarbonMike
-
14 Years Ago
Post Reply
Like
11
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search