Group: Forum Members
Posts: 5,
Visits: 27
|
I've took my time with every step, followed all the instructions, sanded down, laid 3 coats of resin in total, at the end sprayed clear coat as the instruction. The biggest disappointment for me was that the CF fabric didn't stick proper on to the plastic part so was ruined from there. Waited for the basecoat to become tacky as the instruction, followed the correct mixing percentage on everything but unfortunately I probably didn't do something right, and can't figure it out ...
|