Hi!

A few months ago I've done a project and skinned some plastic parts from under the hood, engine area.

http://www.talkcomposites.com/Uploads/Images/1bcbb114-fc33-411e-bbda-8b39.JPG

I've followed all the instructions but for me the basecoat didn't work at all and it didn't keep the CF fabric on the part at all. As I was applying the resin, the CF just came off from the plastic and the final part doesn't have all the nice lines. My first and only project as I saw that it didn't work on any of the 3 items that I've skinned.

I'm attaching some pictures with how my items ended up from my project:

http://www.talkcomposites.com/Uploads/Images/37967fe8-4e24-46c2-a6c8-2365.JPG http://www.talkcomposites.com/Uploads/Images/1ea5ac7b-ed16-48f3-a787-16d2.JPG http://www.talkcomposites.com/Uploads/Images/395dcf17-697e-45b3-8332-0a2b.JPG

 http://www.talkcomposites.com/Uploads/Images/cf1d180a-e31f-492e-bd29-eda0.JPG http://www.talkcomposites.com/Uploads/Images/5c6201df-6cbd-42ba-8834-44f2.JPG

And the professional items should look something like this:

http://www.talkcomposites.com/Uploads/Images/54215180-b411-4c6c-9769-219a.jpg http://www.talkcomposites.com/Uploads/Images/08869e36-2266-4ada-bdc5-d4a7.jpg

Any idea why the why the CF fabric didn't stick completely on to the plastic and came off as I was applying the resin, why didn't the basecoat hold it proper? Should I have left the CF fabric on to the base coat longer to glue proper?