I have been making laminates using Linnen material and EC laminating epoxy and it works OK.  I do a hand layup and the squeeze out the excess resin in a press.  The thickness is 25mm and the max size about 200mm x 50mm

I would like to try a resin that is water clear and UV stable such as EC Polyurethane casting resin.

Is Easy Composites Polyurethane resin suitable for this application or is there anything else suitable?

I suspect that I wont have long enough to work unless the resin is thin enough to soak through a ready made stack of cloth.  I would also like to know if the resin will stay in the laminate, is it so thin it will all run out leaving it dry?

Thanks

Mike

Edit.  I am not keen on using polyester as I will be working in our kitchen and wifey no likey the smellySmile
Edited 11 Years Ago by pieinthesky
Reply
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
Our WaterclearPolyurethane Casting Resin is primarily designed as a casting not laminating resin.

In principle it will wet out the fabric much like any other resin.  How much would remain is difficult to say.  It is quite a thin resin compared to most laminating resins so i would expect a lot more to naturally run out than with another system.  How that would perform when compressed in a mould is difficult to say!

Also the potlife is only 12-17 minutes meaning you'd need to work fast!!


Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant