From what I've seen (but not tried yet) Polyurethane resins react more to impurities, water, wood etc creating bubbles within the resin so it would not be suitable for lamination.
I'm looking at casting sections of pure PU for my next project but from others experiences it has to be 2-5min cure to prevent the bubbles forming, i.e. it has to cure before it has time to react
|