Hi i am about to try out the chemical "easy lease" release agent.
In the application instructions on the website it recommends 6 coats for new molds.
Mine  are old molds that have been cleaned of all the old wax.
Do i still need 6 coats on these old molds?
Reply
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
Here you go:

Lint Free Solvent Application Wipes

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant