PVA only or PVA + Wax?


Author
Message
StanTheMan
StanTheMan
Supreme Being (455 reputation)Supreme Being (455 reputation)Supreme Being (455 reputation)Supreme Being (455 reputation)Supreme Being (455 reputation)Supreme Being (455 reputation)Supreme Being (455 reputation)Supreme Being (455 reputation)Supreme Being (455 reputation)
Group: Forum Members
Posts: 61, Visits: 380
I'm about to do my first mould and I'm not sure if I should just use PVA release agent only or I should combine it with release wax. Surface finish isn't of much importance as I will be polishing the mould after anyway. Would I get away with PVA only or should I do PVA and then wax that?

Regards,
Stan
Reply
carbonfibreworks
carbonfibreworks
Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)
Group: Forum Members
Posts: 292, Visits: 4.5K
Its down to choice but i never use PVA or wax as i use a chemical release and to date have not had a part stick.
Chris
carbonfibreworks.co.uk

http://www.talkcomposites.com/Uploads/Images/97e08777-693c-4af1-a27a-86cf.png
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search