PVA only or PVA + Wax?

http://www.talkcomposites.com/Topic8976.aspx

By StanTheMan - 12/29/2013 6:32:11 PM

I'm about to do my first mould and I'm not sure if I should just use PVA release agent only or I should combine it with release wax. Surface finish isn't of much importance as I will be polishing the mould after anyway. Would I get away with PVA only or should I do PVA and then wax that?

Regards,
Stan
By ajb100 - 12/29/2013 7:34:04 PM

Best combination I've found is multiple coats of easy lease with a coat of buffed wax after to give the final gloss