Both the EC EL2 and IN2 seems to be almost water-clear (no yellow tint, that I can discern) West Systems "Normal" Resin and Hardener is the same, but their "Coating Hardener" has a distinct yellow tint, something to do with the UV resistance I think.
Maybe the German stuff you have is UV-stabilized coating Epoxy? which could explain the yellow tint.
Also I found that West systems hardener gets more yellow with age, but then we are talking several years storage in varying conditions.. Cool and dark storage is a must for any Epoxy system components. West systems have gone back to using metal cans, since that removes most of the problem of light affecting the long term storage of the resin or hardener.
I keep all my Epoxy resins in one closed cupboard, and all hardeners in a separate closed but ventilated cupboard.
"Sapere Aude"... Dare to KNOW!
The written word is the only truly efficient vehicle for transmitting a complex concept from mind to mind...