Ok so I have resisted doing the tub as its a huge amount of work... Ive made moulds and composite panels for the Front & rear clams, doors and front wings.... I wrapped the roof and window panels on the Tub which looked ok but not perfect and there was clearly no benefit other than cosmetics and it never really sat right with me.... I felt I had left the car unfinished!

So I have striped the car completely, sent the engine for a check over (ready for more power next year) and have been sanding the tub ready to start making the moulds.

Im not going to rush this project and I will need to make an oven to properly post cure it... Im also overseas with work around 5 weeks over the next few months so progress will be slow... but i will try to update this thread with picks to show process/progress.







roof is carbon wrapped with a v weave... its not perfect and didn't save weight.

Edited 12 Years Ago by andygtt
Replies
Shaneer22
Shaneer22
Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)
Group: Forum Members
Posts: 156, Visits: 14K
Nice work,you must have been ready to fall over with fumes using unimold, a very god system especially for polishing up I only use during summer when I can work out side ,I seem to have a low tolerance to polyesters resin.god luck.
andygtt
andygtt
Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)
Group: Forum Members
Posts: 157, Visits: 1.2K
Shaneer22 (07/01/2014)
Nice work,you must have been ready to fall over with fumes using unimold, a very god system especially for polishing up I only use during summer when I can work out side ,I seem to have a low tolerance to polyesters resin.god luck.


I've had some issues before so I use a mask now :-)
Edited 11 Years Ago by andygtt
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
andygtt - 12 Years Ago
ajb100 - 12 Years Ago
FLD - 12 Years Ago
matthieutje65 - 12 Years Ago
Warren (Staff) - 12 Years Ago
wojtepanik - 12 Years Ago
andygtt - 12 Years Ago
wojtepanik - 12 Years Ago
FLD - 12 Years Ago
Warren (Staff) - 12 Years Ago
FLD - 12 Years Ago
andygtt - 12 Years Ago
Warren (Staff) - 12 Years Ago
pk_090 - 12 Years Ago
andygtt - 12 Years Ago
andygtt - 12 Years Ago
andygtt - 12 Years Ago
Warren (Staff) - 12 Years Ago
andygtt - 12 Years Ago
Warren (Staff) - 12 Years Ago
FLD - 12 Years Ago
andygtt - 12 Years Ago
Warren (Staff) - 12 Years Ago
FLD - 12 Years Ago
andygtt - 12 Years Ago
Warren (Staff) - 11 Years Ago
andygtt - 11 Years Ago
wildcard - 11 Years Ago
Warren (Staff) - 11 Years Ago
matthieutje65 - 11 Years Ago
wildcard - 11 Years Ago
Shaneer22 - 11 Years Ago
andygtt - 11 Years Ago
andygtt - 11 Years Ago
wildcard - 11 Years Ago
Hanaldo - 11 Years Ago
andygtt - 11 Years Ago
ajb100 - 11 Years Ago
Hanaldo - 11 Years Ago
matthieutje65 - 11 Years Ago
andygtt - 11 Years Ago
wildcard - 11 Years Ago
andygtt - 11 Years Ago
wildcard - 11 Years Ago
wozza - 11 Years Ago
     what is GC50?
andygtt - 11 Years Ago
Warren (Staff) - 11 Years Ago
andygtt - 11 Years Ago
Matt (Staff) - 11 Years Ago
andygtt - 11 Years Ago
wildcard - 11 Years Ago
bewbzout - 11 Years Ago
FLD - 11 Years Ago
andygtt - 11 Years Ago
     Beautiful.
Hanaldo - 11 Years Ago
andygtt - 11 Years Ago
TomDesign - 11 Years Ago
Warren (Staff) - 11 Years Ago
Alibro - 11 Years Ago
BlackNDecker - 11 Years Ago
ajb100 - 11 Years Ago
BlackNDecker - 11 Years Ago
Hanaldo - 11 Years Ago
BlackNDecker - 11 Years Ago
Hanaldo - 11 Years Ago
Warren (Staff) - 11 Years Ago
Hanaldo - 11 Years Ago
andygtt - 11 Years Ago
Hanaldo - 11 Years Ago
FLD - 11 Years Ago
Hanaldo - 11 Years Ago
FLD - 11 Years Ago
macgtech - 11 Years Ago
andygtt - 11 Years Ago
uniquesc - 11 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search