Ok so I have resisted doing the tub as its a huge amount of work... Ive made moulds and composite panels for the Front & rear clams, doors and front wings.... I wrapped the roof and window panels on the Tub which looked ok but not perfect and there was clearly no benefit other than cosmetics and it never really sat right with me.... I felt I had left the car unfinished!

So I have striped the car completely, sent the engine for a check over (ready for more power next year) and have been sanding the tub ready to start making the moulds.

Im not going to rush this project and I will need to make an oven to properly post cure it... Im also overseas with work around 5 weeks over the next few months so progress will be slow... but i will try to update this thread with picks to show process/progress.







roof is carbon wrapped with a v weave... its not perfect and didn't save weight.

Edited 12 Years Ago by andygtt
Reply
andygtt
andygtt
Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)
Group: Forum Members
Posts: 157, Visits: 1.2K
pk_090 (12/12/2013)
Haven't posted on this forum in a loooooon time but i think this is really worthy. I love what you are doing here Andy! What engine specs are you going for?
Also just to add this spanner to the works, a friend of mine works for the company that provides f1 teams with their pre-preg. He told me that red bull racing cam covers were 1 layer thick of normal pre-preg carbon. Obviously i can say this is 100% accurate but i can see why they do it!

Alex


glad you like it, and thanks for the info... the engine is already 700bhp, its unique in the UK as its a single turbo that I designed myself with my own design of clutch package.... car is a real 1off in almost all areas.

To be honest all the mods on this car is simply R&D for my scratch build car that I have designed and been building forever lol.
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
andygtt - 12 Years Ago
ajb100 - 12 Years Ago
FLD - 12 Years Ago
matthieutje65 - 12 Years Ago
Warren (Staff) - 12 Years Ago
wojtepanik - 12 Years Ago
andygtt - 12 Years Ago
wojtepanik - 12 Years Ago
FLD - 12 Years Ago
Warren (Staff) - 12 Years Ago
FLD - 12 Years Ago
andygtt - 12 Years Ago
Warren (Staff) - 12 Years Ago
pk_090 - 12 Years Ago
andygtt - 12 Years Ago
andygtt - 12 Years Ago
andygtt - 12 Years Ago
Warren (Staff) - 12 Years Ago
andygtt - 12 Years Ago
Warren (Staff) - 12 Years Ago
FLD - 12 Years Ago
andygtt - 12 Years Ago
Warren (Staff) - 12 Years Ago
FLD - 12 Years Ago
andygtt - 12 Years Ago
Warren (Staff) - 11 Years Ago
andygtt - 11 Years Ago
wildcard - 11 Years Ago
Warren (Staff) - 11 Years Ago
matthieutje65 - 11 Years Ago
wildcard - 11 Years Ago
Shaneer22 - 11 Years Ago
andygtt - 11 Years Ago
andygtt - 11 Years Ago
wildcard - 11 Years Ago
Hanaldo - 11 Years Ago
andygtt - 11 Years Ago
ajb100 - 11 Years Ago
Hanaldo - 11 Years Ago
matthieutje65 - 11 Years Ago
andygtt - 11 Years Ago
wildcard - 11 Years Ago
andygtt - 11 Years Ago
wildcard - 11 Years Ago
wozza - 11 Years Ago
     what is GC50?
andygtt - 11 Years Ago
Warren (Staff) - 11 Years Ago
andygtt - 11 Years Ago
Matt (Staff) - 11 Years Ago
andygtt - 11 Years Ago
wildcard - 11 Years Ago
bewbzout - 11 Years Ago
FLD - 11 Years Ago
andygtt - 11 Years Ago
     Beautiful.
Hanaldo - 11 Years Ago
andygtt - 11 Years Ago
TomDesign - 11 Years Ago
Warren (Staff) - 11 Years Ago
Alibro - 11 Years Ago
BlackNDecker - 11 Years Ago
ajb100 - 11 Years Ago
BlackNDecker - 11 Years Ago
Hanaldo - 11 Years Ago
BlackNDecker - 11 Years Ago
Hanaldo - 11 Years Ago
Warren (Staff) - 11 Years Ago
Hanaldo - 11 Years Ago
andygtt - 11 Years Ago
Hanaldo - 11 Years Ago
FLD - 11 Years Ago
Hanaldo - 11 Years Ago
FLD - 11 Years Ago
macgtech - 11 Years Ago
andygtt - 11 Years Ago
uniquesc - 11 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search