Carbon Tub for Noble


Author
Message
andygtt
andygtt
Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)
Group: Forum Members
Posts: 157, Visits: 1.2K
Ok so I have resisted doing the tub as its a huge amount of work... Ive made moulds and composite panels for the Front & rear clams, doors and front wings.... I wrapped the roof and window panels on the Tub which looked ok but not perfect and there was clearly no benefit other than cosmetics and it never really sat right with me.... I felt I had left the car unfinished!

So I have striped the car completely, sent the engine for a check over (ready for more power next year) and have been sanding the tub ready to start making the moulds.

Im not going to rush this project and I will need to make an oven to properly post cure it... Im also overseas with work around 5 weeks over the next few months so progress will be slow... but i will try to update this thread with picks to show process/progress.







roof is carbon wrapped with a v weave... its not perfect and didn't save weight.

Edited 12 Years Ago by andygtt
Replies
andygtt
andygtt
Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)
Group: Forum Members
Posts: 157, Visits: 1.2K
Ok cheers Warren, in that case I have tried GC50 and have some on the shelf.... the reason I don't use that on larger parts at all is that if you have an issue then its scrap as you see the air / pinholes trapped behind the gel coat which is impossible to rectify.

My tub has pinholes because the back wasn't full vacuum, however this is being rectified when its lacquered.... Its at the paint shop as I type and hopefully I should get it back tomorrow and will post more pics then.
Matt (Staff)
Matt (Staff)
Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)
Group: Forum Members
Posts: 680, Visits: 1.9K
Inspiring stuff as ever Andy. Thank you so much for posting your progress on the forum, it's a real world example of what can be acheived if you're determined enough. Sure not everything goes perfectly to plan but I like to think that between us we find a way through each time and the results are stunning.

Paul, me or both of us would definately like to take a run over and film some sort of segment on the project as it nears completion. Really, I'd like to take lots of shots but Staffs to Suffolk is a fair run so it might have to wait until the end.

I'm sure we'll talk again very soon!

Matt Statham
Easy Composites / Carbon Mods - Technical Sales
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
andygtt - 12 Years Ago
ajb100 - 12 Years Ago
FLD - 12 Years Ago
matthieutje65 - 12 Years Ago
Warren (Staff) - 12 Years Ago
wojtepanik - 12 Years Ago
andygtt - 12 Years Ago
wojtepanik - 12 Years Ago
FLD - 12 Years Ago
Warren (Staff) - 12 Years Ago
FLD - 12 Years Ago
andygtt - 12 Years Ago
Warren (Staff) - 12 Years Ago
pk_090 - 12 Years Ago
andygtt - 12 Years Ago
andygtt - 12 Years Ago
andygtt - 12 Years Ago
Warren (Staff) - 12 Years Ago
andygtt - 12 Years Ago
Warren (Staff) - 12 Years Ago
FLD - 12 Years Ago
andygtt - 12 Years Ago
Warren (Staff) - 12 Years Ago
FLD - 12 Years Ago
andygtt - 12 Years Ago
Warren (Staff) - 11 Years Ago
andygtt - 11 Years Ago
wildcard - 11 Years Ago
Warren (Staff) - 11 Years Ago
matthieutje65 - 11 Years Ago
wildcard - 11 Years Ago
Shaneer22 - 11 Years Ago
andygtt - 11 Years Ago
andygtt - 11 Years Ago
wildcard - 11 Years Ago
Hanaldo - 11 Years Ago
andygtt - 11 Years Ago
ajb100 - 11 Years Ago
Hanaldo - 11 Years Ago
matthieutje65 - 11 Years Ago
andygtt - 11 Years Ago
wildcard - 11 Years Ago
andygtt - 11 Years Ago
wildcard - 11 Years Ago
wozza - 11 Years Ago
     what is GC50?
andygtt - 11 Years Ago
Warren (Staff) - 11 Years Ago
andygtt - 11 Years Ago
Matt (Staff) - 11 Years Ago
andygtt - 11 Years Ago
wildcard - 11 Years Ago
bewbzout - 11 Years Ago
FLD - 11 Years Ago
andygtt - 11 Years Ago
     Beautiful.
Hanaldo - 11 Years Ago
andygtt - 11 Years Ago
TomDesign - 11 Years Ago
Warren (Staff) - 11 Years Ago
Alibro - 11 Years Ago
BlackNDecker - 11 Years Ago
ajb100 - 11 Years Ago
BlackNDecker - 11 Years Ago
Hanaldo - 11 Years Ago
BlackNDecker - 11 Years Ago
Hanaldo - 11 Years Ago
Warren (Staff) - 11 Years Ago
Hanaldo - 11 Years Ago
andygtt - 11 Years Ago
Hanaldo - 11 Years Ago
FLD - 11 Years Ago
Hanaldo - 11 Years Ago
FLD - 11 Years Ago
macgtech - 11 Years Ago
andygtt - 11 Years Ago
uniquesc - 11 Years Ago