Hello,

I a newbie here. Sorry for my poor english, I hope It will be clear.

Do you guys have any idea how to prepare molds and vacuum bags to perform resin infusion on my 2-parts mould?
Imagine my part - is is like a tube, but its profile is not just a circle but something like epllipse.
What I need is to get  uniform part, staight from my 2 - parts mould, in one piece Wink
Should I build a special mold? 
It is posible to set vacum bags up to make it posible? Or do I need to glue two seperately made parts?

Thanks for you help!

Peter
Reply
Matthieu Libeert
Matthieu Libeert
Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
The thing you are trying to do is a technique called 'bladder moulding' check it on google and youtube... you should find some inspiration and some information on how to make/prepare your moulds. Its done with pressure instead of vacuum

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search