How to set this mold up?


Author
Message
Brian_s
Brian_s
Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)
Group: Forum Members
Posts: 99, Visits: 2.5K
Something like this may give you some pointers.

http://www.youtube.com/watch?v=Vbe0eAxMzPE

Brian.
_pepis
_pepis
Forum Member (27 reputation)Forum Member (27 reputation)Forum Member (27 reputation)Forum Member (27 reputation)Forum Member (27 reputation)Forum Member (27 reputation)Forum Member (27 reputation)Forum Member (27 reputation)Forum Member (27 reputation)
Group: Awaiting Activation
Posts: 5, Visits: 47
Hello,
Thank you very much! This is what I was looking for.

Now few question how to prepare 2 halfs (moulds) to have them glued together.
I suppose they must be perfectly sealed, and all my fibres cut at the edge of the mould?

Thank you!
Matthieu Libeert
Matthieu Libeert
Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
The thing you are trying to do is a technique called 'bladder moulding' check it on google and youtube... you should find some inspiration and some information on how to make/prepare your moulds. Its done with pressure instead of vacuum

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




_pepis
_pepis
Forum Member (27 reputation)Forum Member (27 reputation)Forum Member (27 reputation)Forum Member (27 reputation)Forum Member (27 reputation)Forum Member (27 reputation)Forum Member (27 reputation)Forum Member (27 reputation)Forum Member (27 reputation)
Group: Awaiting Activation
Posts: 5, Visits: 47
Hello,

1. - is what I'd like to get as uniform shape. it is around 80 cm long and 8 cm wide. Empty inside, kind of a tube

2. - This is how I make it now. I have 2 parts (yellow+black on my pic) and glue them thogether wich is very difficult.

I've seen on this movie http://www.youtube.com/watch?v=504I_hJDFck#t=304 (interesing, BTW) they make a tube (car part) in two parts mold.

Thanks in advance!

Peter
http://www.talkcomposites.com/Uploads/Images/95cc5913-97d1-48b4-8353-4487.jpg
wozza
wozza
Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)
Group: Forum Members
Posts: 688, Visits: 5.4K
Hi, some pictures or drawings of the part you want to make will make it easier to give advice/ideas.

Warren

Carbon Copies Ltd
_pepis
_pepis
Forum Member (27 reputation)Forum Member (27 reputation)Forum Member (27 reputation)Forum Member (27 reputation)Forum Member (27 reputation)Forum Member (27 reputation)Forum Member (27 reputation)Forum Member (27 reputation)Forum Member (27 reputation)
Group: Awaiting Activation
Posts: 5, Visits: 47
Hello,

I a newbie here. Sorry for my poor english, I hope It will be clear.

Do you guys have any idea how to prepare molds and vacuum bags to perform resin infusion on my 2-parts mould?
Imagine my part - is is like a tube, but its profile is not just a circle but something like epllipse.
What I need is to get  uniform part, staight from my 2 - parts mould, in one piece Wink
Should I build a special mold? 
It is posible to set vacum bags up to make it posible? Or do I need to glue two seperately made parts?

Thanks for you help!

Peter
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search