laminating resin as gelcoat


Author
Message
japcarmaniac
japcarmaniac
Supreme Being (401 reputation)Supreme Being (401 reputation)Supreme Being (401 reputation)Supreme Being (401 reputation)Supreme Being (401 reputation)Supreme Being (401 reputation)Supreme Being (401 reputation)Supreme Being (401 reputation)Supreme Being (401 reputation)
Group: Forum Members
Posts: 53, Visits: 157
can a coat of laminating resin be used as a first coat of a mould? the smell of the polyester is driving me nuts and was going to try the epoxy resin instead.

thanks


Reeday
Reeday
Junior Member (7 reputation)Junior Member (7 reputation)Junior Member (7 reputation)Junior Member (7 reputation)Junior Member (7 reputation)Junior Member (7 reputation)Junior Member (7 reputation)Junior Member (7 reputation)Junior Member (7 reputation)
Group: Awaiting Activation
Posts: 1, Visits: 3
What you will find when trying to use laminating resin as a gelcoat is that it will fish eye when brushed on due to the release agent. Easy composites do a clear colourless Epoxy Gel coat which will work alot better. If your going down the gelcoat route, try to get as thinner film on as possible, spraying it on with a dump/cup gun will give you the best results.
kylle
kylle
Supreme Being (306 reputation)Supreme Being (306 reputation)Supreme Being (306 reputation)Supreme Being (306 reputation)Supreme Being (306 reputation)Supreme Being (306 reputation)Supreme Being (306 reputation)Supreme Being (306 reputation)Supreme Being (306 reputation)
Group: Forum Members
Posts: 34, Visits: 101
Its possible to spray clear gelcoat wht a small air gun *question mark.... I.m having problems wht my keyboard sorry!!! 
MAVERICK
MAVERICK
Supreme Being (251 reputation)Supreme Being (251 reputation)Supreme Being (251 reputation)Supreme Being (251 reputation)Supreme Being (251 reputation)Supreme Being (251 reputation)Supreme Being (251 reputation)Supreme Being (251 reputation)Supreme Being (251 reputation)
Group: Forum Members
Posts: 27, Visits: 39
I've tried spraying spray-gel with a conventional HVLP spray gun... I have to say the results were not great! basically it only just barely came out! That was with a 1.6mm nozzle, looking at the gear like cup-guns they seem to have pretty huge nozzles... I'm sure that's where the answer lies.
mhdghoul
mhdghoul
Supreme Being (447 reputation)Supreme Being (447 reputation)Supreme Being (447 reputation)Supreme Being (447 reputation)Supreme Being (447 reputation)Supreme Being (447 reputation)Supreme Being (447 reputation)Supreme Being (447 reputation)Supreme Being (447 reputation)
Group: Forum Members
Posts: 49, Visits: 113
yup u can i do that all the time in fact i prefer it cause the gelcoat isnt as clear as the resin but make sure u put 2 layers of pva and puff your wax perfectly before the pva , i always do that and if your mold is good u wouldnt need to do anything to the part cause it will release shiny tooSmile

best regards mhd alghoul mhdghoul@hotmail.com youtube channel :atmospherejo link is http://www.youtube.com/user/atmospherejo?ob=0&feature=results_main