By japcarmaniac - 2/26/2012 10:19:23 PM

can a coat of laminating resin be used as a first coat of a mould? the smell of the polyester is driving me nuts and was going to try the epoxy resin instead.

thanks
By mhdghoul - 3/15/2012 9:40:42 PM

yup u can i do that all the time in fact i prefer it cause the gelcoat isnt as clear as the resin but make sure u put 2 layers of pva and puff your wax perfectly before the pva , i always do that and if your mold is good u wouldnt need to do anything to the part cause it will release shiny tooSmile