aran01
aran01
posted 12 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 8,
Visits: 30
Hi folks, As the winter is here now what is the lowest recommended curing temp for EL2 & IN2.
It is currently dropping down to 6degC here in my shed and I was wondering if the resin will eventually cure at this temp?
Kind regards,
aran01
Reply
Like
3
Reply
Matthieu Libeert
Matthieu Libeert
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 955,
Visits: 3.4K
Like everyone says, don't make parts under 15°C or I would even say 20°C
as a small remark I would like to add that low temperatures can be in you favour as well!
https://www.youtube.com/watch?v=V3rAx7LrL0g
This was the first project I did with polyester and flaxfiber, and specially chose to work outside so I would have an unlimited time to work with the polyester.
A lot of polyester was used and I worked for a few hours outside without having any problems, once everything was bagged and inside it started to cure when it got to room temperature.
Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
curing temp
aran01
-
12 Years Ago
You MUST keep it around 20C if you want a successful cure. if you are lucky you might get away with...
Warren (Staff)
-
12 Years Ago
What unused to do before getting my workshop sorted was infuse outside in the cold, then clamp the...
ajb100
-
12 Years Ago
Can you heat the shed? How can you work in 6 degrees anyway? Alternatively, find a place to work...
baja_patient
-
12 Years Ago
Build a warm box for your resin and cloth, doesn't need to be much just an MDF box with a low...
ChrisR
-
12 Years Ago
Thanks guys for the feedback. I am working with a heater but I am moving the parts indoors once...
aran01
-
12 Years Ago
Last winter I made some parts that latterly 1mth later still hadn't cured... I found if it didn't...
andygtt
-
12 Years Ago
Like everyone says, don't make parts under 15°C or I would even say 20°C as a small remark I would...
matthieutje65
-
12 Years Ago
[quote][b]andygtt (21/11/2013)[/b][hr]Last winter I made some parts that latterly 1mth later still...
stuart321
-
12 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search