			            Hey guys, I cant go ahead with one problem , I infuse my parts everything is good quality , I cure them in oven but my finished surface has signs of carbon fiber.. Is it possible to fight against this without using gelcoat?
  Last time for instance when I used lantor soric on flat sheet it also could be seen in some angles on finished product.. I could even feel it under my fingers
  The funny thing its not seen in photos.
 
  I start to think that this issue is the biggest disadvantage of using infusion process.