By fiberpro - 8/30/2013 10:02:11 AM
Hey guys, I cant go ahead with one problem , I infuse my parts everything is good quality , I cure them in oven but my finished surface has signs of carbon fiber.. Is it possible to fight against this without using gelcoat?
Last time for instance when I used lantor soric on flat sheet it also could be seen in some angles on finished product.. I could even feel it under my fingers
The funny thing its not seen in photos.
I start to think that this issue is the biggest disadvantage of using infusion process.
Whats your ideas?
|
By fiberpro - 8/30/2013 4:29:35 PM
Mould is made from epoxy. It is said it's hardener for 180minutes life, but of course oven curing shorten this time. I test it on small flat panels like 30x40 centimeters, so its not a big thing I guess
|
|