Can anyone tell me the best way to cut aluminium core? We use water jet to cut core and CNC machine to mill it. But i was looking for a manual method. I have tried desouter (diamond) cutter but it simply melts down the metal. I have also tried bandsaw cutter which gives a good finish but very difficult to control the tolerances.

Any Brighter Ideas??

Reply
wozza
wozza
Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)
Group: Forum Members
Posts: 688, Visits: 5.4K
mirfu101 (28/08/2013)
wozza (28/08/2013)

One method I have used in the past is to clamp the core between two pieces of thin (3-6mm)  MDF. You can then mark out the shape you want onto that and cut it with a jigsaw or bandsaw. Cutting through the MDF and the core at the same time stops the blade wondering.

Warren
 
 
The problem in fibre board or Dam to cut through in bandsaw is that it aint feasible for high production rate. I might need to use lots of MDF for each of the aluminium core to be cut.


Are you cutting the same sized pieces? If so cut the MDF to size and use it as a template. Using the edge of the MDF as a guide for the blade. Just an idea that may be worth trying.Smile

Warren

Carbon Copies Ltd
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search