Unimould - Veins of coupling coat through gelcoat
Unimould - Veins of coupling coat through gelcoat
Post Reply
Like
3
Unimould - Veins of coupling coat through gelcoat
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
LaxFriedrichs
LaxFriedrichs
posted 12 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 58,
Visits: 450
After sanding down the mould to remove the edging marks of the release tape there is the odd 'vein' (more capillary) of coupling coat coming through the gelcoat. There maybe two on the whole mould, so I'd imagine the gelcoat thickness, overall, is fit for purpose?
Can these be ignored, or must I repair? For the repair, do I take a small very shallow divot on the vein, fill with gelcoat, and sand over. It's time consuming, so if I can ignore it I will...
Cheers!
Reply
Like
3
Reply
carbonfibreworks
carbonfibreworks
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 292,
Visits: 4.5K
I have had the same situation caused by not having the correct thickness of gelcoat, I used easy lease on the moulds and had no issues.
Chris
www.carbonfibreworks.co.uk
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Unimould - Veins of coupling coat through gelcoat
LaxFriedrichs
-
12 Years Ago
I have had the same situation caused by not having the correct thickness of gelcoat, I used easy...
carbonfibreworks
-
12 Years Ago
Thanks :)
LaxFriedrichs
-
12 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search