After sanding down the mould to remove the edging marks of the release tape there is the odd 'vein' (more capillary) of coupling coat coming through the gelcoat. There maybe two on the whole mould, so I'd imagine the gelcoat thickness, overall, is fit for purpose?

Can these be ignored, or must I repair? For the repair, do I take a small very shallow divot on the vein, fill with gelcoat, and sand over. It's time consuming, so if I can ignore it I will...

Cheers!
carbonfibreworks
carbonfibreworks
Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)
Group: Forum Members
Posts: 292, Visits: 4.5K
I have had the same situation caused by not having the correct thickness of gelcoat, I  used easy lease on the moulds and had no issues.

Chris

www.carbonfibreworks.co.uk

http://www.talkcomposites.com/Uploads/Images/97e08777-693c-4af1-a27a-86cf.png
LaxFriedrichs
LaxFriedrichs
Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)
Group: Forum Members
Posts: 58, Visits: 450
Thanks Smile
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search