Hey guys, just finally got done getting all the peelply and godamn mesh out of the part. I made I bit resin rich cos I was trying some things out. Well the part came out great and pinhole free.

The downside is getting that stuff out. Sticks like s*** to blanket to be honest.

I read somewhere quite a while ago though, that you can put a layer of perforated release film between peelply and mesh? would this work, has anyone tried this?


cheers
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search