By baja_patient - 7/21/2013 1:15:13 AM
Hey guys, just finally got done getting all the peelply and godamn mesh out of the part. I made I bit resin rich cos I was trying some things out. Well the part came out great and pinhole free.
The downside is getting that stuff out. Sticks like s*** to blanket to be honest.
I read somewhere quite a while ago though, that you can put a layer of perforated release film between peelply and mesh? would this work, has anyone tried this?
cheers
|
By Warren (Staff) - 7/22/2013 11:44:21 AM
perforated release film will work for this purpose. Just slow the infusion slightly as it takes a bit longer to filter through the film.